BÖHLER N352S1 is a martensitic chromium steel with nickel addition. Heat treatable grade, capable of taking a mirror finish. Higher corrosion resistance compared to 13% chromium steel. Resistant to the effects of seawater, weak acids and alkaline solutions, as well as to acids having a strong, oxidizing effect such as nitric acid. Surface finish for optimum corrosion resistance: fine ground or polished.
For components subject to high mechanical and corrosive stress, e.g. screws and shafts, at operating temperatures up to approx. 752° F.
Martensitic chromium steel with nickel addition. Heat treatable grade, capable of taking a mirror finish. Resistant to the effects of seawater, weak acids and alkaline solutions, as well as to acids having a strong, oxidizing effect such as nitric acid. Surface finish for optimum corrosion resistance: fine ground or polished.
Market grade | EN |
---|---|
431 | X15CrNi17-3 |
BS |
---|
S80 |
C | Si | Mn | P | S | Cr | Mo | Ni | V | W | Cu | Co | Ti | Nb | Fe | Sn | |
---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|
0.12 to 0.2 | max. 1 | max. 1 | max. 0.03 | max. 0.025 | 15 to 18 | max. 0.3 | 2 to 3 | max. 0.2 | max. 0.05 | max. 0.3 | max. 0.05 | max. 0.05 | max. 0.05 | REM | max. 0.02 |
Information on Long Products ) Presented data refer exclusively to long products. Please observe the detailed explanations at the end of the data sheet (pdf).
Contact Bohler UK about anything related to our products and services and we will get back to you.